Your Question is very generic.

It depends on the Code, Specification, and Application.

For eg if the Code is ASME Sec.IX and the pipe is SA106Gr.B & the Flange is SA105, then P.No & Group No of pipe will be P1 & Gr.1 Whereas Flange will be P1 & Gr.2.

If you Qualify P1 Gr.1 to P1 Gr2, then it qualifies P1Gr1 to P1Gr1 and P1Gr2 to P1Gr2 & P1Gr1 to P1Gr2.

See below snap shot from ASME Sec.iX

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 6 December, 2023 at 11:08:22 am IST, Muhammed Shareef <shareefpyari@gmail.com> wrote:


Dear experts,

Is it mandatory to qualify PQR with pipe and flange.? Why can't we qualify with pipe only. What is the limitations here to do so.


Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2iHPvcgmWqje6V5d4g8iojz_p%3DXHmB7LCHG2vfQWbzUs33GA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...