Normally either from the Process or Mechanical Designer will provide the MDMT ( Minimum Design Metal Temperature) - it is the lowest temperature attained by the Material either due to Process conditions / Environmental conditions / upset conditions. So Impact testing has to be performed at MDMT.

Charpy Impact values for Full size specimen (10x10x55) will be specified either by the Design Code  or superceded by the Client specification if provided. Test Temperature MDMT.

A Snap shot of ASME B 31.3 is given as example below.

Inline image

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 6 December, 2023 at 09:34:42 am IST, Prathamesh Patkar <prathameshpatkar@swastikindustriesindia.in> wrote:


Dear Sir,

Thank you for the response.

I had one more query. Are there any acceptance criteria for minus temperature? eg... the specimen should sustain 12 J impact at -20c in order to qualify. 



On Mon, Dec 4, 2023 at 5:30 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
A Charpy Impact test is not required for specimen thickness less than 2.5mm.

Subsize specimens can be machined from the Pipe OD 60mm and thickness 5.5mm. Please check with the Mechanical testing lab.

Please refer to ASME Sec.IIA section SA-370.

If specimen thickness exceeds 80% during machining from the original size, temperature reduction according to the Applicable Code shall be applied.

For subsize specimens Impact values refer to snap shot.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Monday, 4 December, 2023 at 05:06:28 pm IST, Prats <prathameshpatkar@swastikindustriesindia.in> wrote:


Hello,

We have an impact testing requirement to be done on a pipe with an outer diameter of 60mm and a thickness of 5.5mm. 

What specimen size should we select for the testing? As the standard "ASTM E23-23A" states, specimen size should be 55L x 10W x 10 thick. We are a bit confused regarding the specimen size...has anyone faced a similar issue? please recommend 

Moreover, the specimen should sustain 27 J. 

Please help.

Thanks & Regards 
Prats

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d6ea2566-4818-419b-9dcf-d307c61bab53n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/598336985.6110574.1701690837182%40mail.yahoo.com.


--

Regards,




--
Thanks & Regards
Prathamesh S Patkar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC4daO1FWBtE5gfLNgNYqhsVg%2Bu0V475C3r53uDxgj82GDtq8A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...