Wednesday, December 6, 2023

Re: [MW:34684] How to select WPS Electrical parameters

PQR is result of WPS


On Wed, 6 Dec 2023 at 8:38, Muhammed Shareef
<shareefpyari@gmail.com> wrote:
Dear team,

Can anyone clarify me ,

How we decide the electrical parameters of WPS. Will it be the same as PQR or what is the limit. 


Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2iHPssh%2BebeDtvBzxFT%2BuXSnJ%3DNcs2hwtUxbFt8V04eC8%2BWQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1229628900.403883.1701858331940%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...