Re: [MW:34677] Impact testing - V NOTCH CHARPY. Recommendation

You can take subsize specimen provided take consideration of thickness reduction 

On Mon, 4 Dec 2023, 17:06 Prats, <prathameshpatkar@swastikindustriesindia.in> wrote:
Hello,

We have an impact testing requirement to be done on a pipe with an outer diameter of 60mm and a thickness of 5.5mm. 

What specimen size should we select for the testing? As the standard "ASTM E23-23A" states, specimen size should be 55L x 10W x 10 thick. We are a bit confused regarding the specimen size...has anyone faced a similar issue? please recommend 

Moreover, the specimen should sustain 27 J. 

Please help.

Thanks & Regards 
Prats

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d6ea2566-4818-419b-9dcf-d307c61bab53n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM02rkfJOX%2Bh7fabb6Vr3VRwojoZk-B2kM%3Ds%3DpxH9U8eoU_wNQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...