Wednesday, December 27, 2023

[MW:34712] Interpass Temperture - Reg

Dear Gents,

In ASME SEC IX, QW 406.3 States " An increase of more than 100°F (55°C) in
the maximum interpass temperature recorded on the
PQR. This variable does not apply for any of the following
conditions:
(a) WPS is qualified with a heat treatment above the
upper transformation temperature."

Please clarify why this variable is not applied to Upper Transformation Temperature Heat Treatment.


Thanks and Regards,
Nirmal Kumar C

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF7xvucqD%3DQ7nw6vfRiGV_rzwTHF%2B2%3DxdHp-2ifkWk0kW79UsQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...