Hi Uma shankar,
1) 6G - welder - No
2) 6GR welder -Yes, TKY -joints are partial penetration groove joints with limited access during welding.
R stands for restriction ring during performance qualification.
3) TKY NDT - Before welding - UT Lamination check.
After Welding- Wet magnetic particle testing & Angle probe-Ultrasonic testing.
4) Repair Rate- Only applicable for Full penetration groove weld & butt weld only (Category A-CategoryA,B,C)
Regards
Vinoth
On Wed, Jul 26, 2023 at 11:48 AM Uma sankar Sankar <umasankar6246@gmail.com> wrote:
Dear Experts--Can 6G qualified welder can weld T,K,Y joints,yes or no.If yes why,if no why.Why only 6GR qualified welder only can weld T K Y JOINTS?What type of NDT required?How to weekly Repair rate of welder.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO8WSnGALirhW4vroU5hACX-VMQLLvxm4FrmX5dEfEMYb1v45g%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbO-YZ3Rgz3YWv-DiYb44Jp87L%3DK%3DiGdrRqcnJtEmDa8YjsYQ%40mail.gmail.com.
Comments