The equivalent ASTM material for EN-10025 - 2 (S275 J2) is ASTM A572 Grade 42. Both materials have a minimum yield strength of 275 MPa, and a minimum tensile strength of 500 MPa. The impact toughness requirements are also similar, with EN-10025 - 2 (S275 J2) requiring a minimum impact energy of 27 J at 20°C, and ASTM A572 Grade 42 requiring a minimum impact energy of 27 J at -10°C.

Here is a table of the equivalent grades for EN-10025 - 2 (S275 J2):

EN GradeASTM Grade
S275 J2A572 Grade 42
S275 J0A572 Grade 44
S275 JRA1011/A1011M


On Fri, Jul 14, 2023 at 8:47 AM Nirmal chandrasekaran <nirmalchandrasekaran352@gmail.com> wrote:
Hi Gents, Good Evening.

I want to confirm the EN-10025 - 2 (S275 J2) with Equivalent ASTM Material. Kindly Provide the Equivalent Grade for the above mentioned EN Grade Material.

Thanks & Regards
Nirmal Kumar C

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF7xvuc47oD1jr4Cx5pAasznpZFRBK_BYtVDZip2guWvKmuqMQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPBV5RyeXQaLn0d8HccRHwzOtYM-VveAN15ybSCb74wBoNo4ZA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...