Thursday, July 6, 2023

[MW:34387] Re: WPS FOR 321H

I need to replace the roof and bottom plate of a tank. I need to select a welding rod that is compatible with 304H-321H steel. Would 347 welding rod work?

On Thursday, 6 July 2023 at 07:28:41 UTC+3 Vishwas Keskar Welding Manager WELDING wrote:
Dear Ashish 

What is service of the equipment ?(Operating temperature ?)?

The ER321  is compatible wire .

for TYP 347/321 base metals -ER 16 8 2 is deployed when the weld need less FN   when operating temperatures  are higher (> 500 Deg C ) 

Thanks 

Vishwas - IWE
International Welding Engineer 


On Wednesday, July 5, 2023 at 9:02:37 PM UTC+5:30 Ashish Chacko wrote:
Dear experts , can anyone share me the wps for 321H.Am getting confused for the selection of filler material, ER347 or ER 16-8-2.Please support .

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fe9c6543-0cd1-4a3e-b46e-280553916e0cn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...