[MW:34452] SPWHT requirement ASME and ARAMCO - Advise


Hello Everyone,

Could you please advise and share your experience regarding SPWHT requirements of material (Plate, Pipe, forging, Fittings and Flanges) for pressure vessels as per ASME and ARAMCO standard. and please elaborate in detail and also mention the reference if possible. 


If you require any further information, please do not hesitate to contact me .

Thanks & Best Regards,

 

Awais Butt

Senior QA/QC Inspection Engineer | QA/QC Department




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG5KMG_4P2uUt4R8fkAgCWZ6LXHgByghh3-vwwOeboujRHKdaA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...