[MW:34404] Re: CLARIFICATION FOR WELD METAL DEPOSITION CHEMICAL ANALYSIS TOLERANCE ON PMI

Please always send your postings to "materials-welding@googlegroups.com", and not on personal emails

The results of the analysis shall meet the requirements of respective SFA classification (ranges or alerday given) by using the acceptable analytical methods (e.g ASTM E1019) capable of determining whether the composition meets the requirements.
PFI ES-42 tolerance are to be used only incase of PMI using portable X-Ray emission 


On Thu, 13 Jul 2023 at 01:01, sam Raja <samraja224@gmail.com> wrote:
Dear Expert,

Is there any reference standard for weld metal deposition chemical element tolerance?. I didn't find any reference from ASME Secii Part-c.



Kind advise me.

Thanks,
Sam-Kuwait 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkVtja8YKJEcKUfM4XBs3dTW0VDgmifeo%2BmFsesUBjB_Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...