Dear Sir,
When welding 304H to 321H stainless steel, we typically use a 347 filler material which contains a stabilized form of stainless steel, and less sensitive to intergranular corrosion, and has a high resistance to oxidation.
Best regards,
Le jeu. 6 juil. 2023 à 06:38, Ashish Chacko <iamashleo007@gmail.com> a écrit :
I need to replace the roof and bottom plate of a tank. I need to select a welding rod that is compatible with 304H-321H steel. Would 347 welding rod work?--On Thursday, 6 July 2023 at 07:28:41 UTC+3 Vishwas Keskar Welding Manager WELDING wrote:Dear AshishWhat is service of the equipment ?(Operating temperature ?)?The ER321 is compatible wire .for TYP 347/321 base metals -ER 16 8 2 is deployed when the weld need less FN when operating temperatures are higher (> 500 Deg C )ThanksVishwas - IWEInternational Welding EngineerOn Wednesday, July 5, 2023 at 9:02:37 PM UTC+5:30 Ashish Chacko wrote:Dear experts , can anyone share me the wps for 321H.Am getting confused for the selection of filler material, ER347 or ER 16-8-2.Please support .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e91d9eb2-1bbb-4a5a-8ef1-147bb0aa5bfen%40googlegroups.com.
![]() |
| |
TAQA MOROCCO is a member of the Abu Dhabi National Energy Company Group of companies. The information contained in this communication is confidential, may be attorney-client privileged, and is intended only for the use of the addressee. It is the property of Abu Dhabi National Energy Company PJSC (TAQA) or one of its affiliates. Unauthorized use, disclosure or copying of this communication or any part thereof is strictly prohibited and may be unlawful. If you have received this communication in error, please notify me immediately by return email and destroy this communication and all copies thereof, including attachments. | ||
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANRRH0KzySvx9JCKm0DwaPdFTT5hkz%3DWnNseHBAPZx3SOFH%3DFQ%40mail.gmail.com.

Comments