[MW:34416] Electrode 308L used for welding

Dear All, 
We used 316L stainless steel pipe to pipe join so we can use 308L electrodes for welding. Please give your suggestion on the use of electrodes reference to  the code.
Also 316L to 304L material joints. can be used for 308L electrodes for welding.
--
Best regards
Umesh Mansute
Cell +917030000306


--