Tuesday, July 11, 2023

[MW:34401] NO6625 TUBE AND NO6625 TUBES - PWHT OF TTJ WELDING

Dear Experts 

Equipment fabrication - Heat Exchanger fabrication - as per ASME SEC VIII DIV 1 - Tube sheet -SB 564 N06625 -66mm thk x 666 mm OD 
Heat exchanger Tubes - SB-444 N06625- 2.108mm X 19.05mmOD 
Welding -Tube to Tube sheet welding 
Joint configuration - Groove and fillet - (2mm X 45 Deg V with 2 mm fillet). Welding Process - GTAW 
Filler Metal - ERNiCrMo3 
PWHT is required for Tube to tube sheet welds  due to Process reasons.
Query - WPS is to be qualified with PWHT - 
1.What would be PWHT Holding temperature and holding time for the above Tube to tube sheet welds? Advice on recommended Heating and cooling rate for PWHT . 
2. What are the cares that needs to be taken to avoid scaling ? 
3. What would be the advice for sequence for Tube expansion ? (Tube Expansion shall be before PWHT OR after PWHT ) .Technical Expert Answer with details -

Any specific care that to be taken while doing PWHT ( to avoid distortion, to avoid scaling  etc )

Thanks 

Vishwas -IWE 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/498246e3-ac55-4dd4-9ea3-1e8155dbe0aan%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...