Friday, September 30, 2022

Re: [MW:33521] Impact Test Requirement : ASME Sec. VIII Div.1

Dear Sir,


Wt will be the test temperature and the acceptance criteria to procure the material.

On Fri, 30 Sept 2022, 7:55 am Pravin Kurade, <pravinkurade@gmail.com> wrote:
Yes impact is required ref UG 84 chart

On Fri, 30 Sep 2022 at 09:08, williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts, 

Please share the Impact Test requirements of SA 516 Gr.70 N , 80 mm thickness with a MDMT of -29 degree C.

Thank You & Regards

Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ7-ZGwD2T5SHytyTQndeSpueg2kxmG%3DJg5S6cKHMspPUg%40mail.gmail.com.
--
Pravinkumar kurade

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM02rkdw2eJee2Sf1V4KdByc1qRjTegFE1N10DqbgxmwLOnOLA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ586Lpb4syCegm9fd6JfLE4QXKM%2BFVkfeaTxdfghKp2Mw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...