[MW:33492] Re: FCAW - Procedure Qualification Test

Dear Experts,
Greetings!!

Anyone knows the reason for very low impact test values on the weld centerline.
Thanks in advance.

Welding Process : FCAW
Material : SA 516 Gr.70 N, 20 mm Thickness
PWHT : 610 ° C ± 10° C, @ 120 Minutes
Tensile, Bend, Macro & Hardness Values are Accepted.
But in the Charpy Impact Test @ -28° C  , Average on WCL is 09 Joule
In HAZ the average is 217 Joule.

Filler Wire Details
K-71T1-C1, AWS A5.20, 1.2 mm Diameter
Impact Values (as per MTC) , Charpy V-Notch -20° C, Avg. 54 J & Min. 27 J

Thank You & Regards
Williams P Wilson
+968-94600828
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ56G%3Djygx%3D3qHSUNM_DP73okXanYu4JhYwfJkyM12Y2bQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...