Re: [MW:33435] QW-407.2

Supplement variable applicable when impact required

On Mon, 5 Sep 2022 at 13:37, Manikandan J <mechmani22@gmail.com> wrote:
Hai,

QW407.2 is a supplementary essential variable.

 Not applicable when an impact test is required

Regards,
Manikandan

On Mon, Sep 5, 2022 at 10:56 AM williams p wilson <williamswilsonp@gmail.com> wrote:
Dear Experts,

QW-407.2 is not applicable when an impact test is required, Please confirm.


Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHBxnQ5oT-m79w8dV_Bjeruvu5qfTPzyY4ouu9Uy%2BaZ5fd76mA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmOCoytFUncdCBhgxta4NayXjRQWA6pseH79B%2Br1qo0-mw%40mail.gmail.com.
--
Pravinkumar kurade

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM02rkdrGX6ofBHxRusitYB9ku8QU7O%2BdetKpiSicGp6uPCnNA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...