[MW:33508] FILLER WIRE FOR SA240 GR 304 TO ENCOALLOY 8800

Dear all,

What is the filler wire for below mentioned PQR

1 SA240 GR.304 TO UNS NO 8800
2. SA240 GR.304 TO UNS NO 8810



Best Regards
Sujit

--