Re: [MW:33420] Ceramic Nozzle 2411, 2413, 2464 meaning and abbreviation need , any one tell the details

Dear Mr.Matheswaran,

This is TIG welding ceramic nozzle, 24 means length of the nozzle and 11 or 13 means thread size or bottom ID of the nozzle.

if you have any doubt you can check http://www.sapindustries.com    

Regards,
Sankaran.SP
Welding & Metallurgy expert
Coimbatore, India. 


On Thursday, 1 September, 2022 at 12:00:05 pm IST, Madheswaran s <madhes.sss@gmail.com> wrote:


Dear Experts, 

Kindly provide  the details about  ceramic Nozzle 2411, 2413, 2464 meaning and abbreviation with full dimensions , how to understand? 

Thanks , I need answes as soon as possible for auditing purpose, so anyone post as possible quickly.

Thanks.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e7cbd3e8-bb9c-4f4d-a3da-a6cfc3674733n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...