verticality : max 1.5 inch , based on pressure vessel design handbook ... it should be in client specification
straightness : i think UW-33 may be used as a guide , shell courses should be in the same level during fabrication
Best Regards ,
ENG. Ahmed Osman
On Wednesday, September 14, 2022 at 10:49:50 a.m. GMT+3, vishal hirde <vishalhirde1988@gmail.com> wrote:
Dear Forum Member's,
-- We are fabricating 9 Meter- Dia Vessel with 27.2 Meter height as per ASME Sec VIII Div-1 at Site.
Query is regarding Verticality / Straightness Check Tolerances.
Pl. Suggest.
Regards,
Vishal Hirde
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACAaqdo21DsvgvD3EJW0ZXRH1XPTdf4rf2bD%3Dzv1Cv6o2dRy8w%40mail.gmail.com.