Monday, September 5, 2022

Re: [MW:33434] Filler rod to weld titanium to SS304

Dear Sir,

Thank you for the input.
How about TIG or MIG process? 

Any solution for such combination welding? 
Because the site project requirement is to join SS304 to Titanium grade 2.

On Mon, 5 Sep 2022 at 16:21, 'Prakash Hegde' via Materials & Welding <materials-welding@googlegroups.com> wrote:
No
You can not weld Ti to any Metal by.Arc. welding process
Regards
On Mon, 5 Sep 2022 at 13:41, Pravin Poornachandran
Dear Expert,

Good day.

Can anyone share which filler to use to weld titanium to stainless steel 304? 

Understand that it's difficult to weld this 2 material considering it's thermal expansion is entirely different. 

Kindly advise.

Best regards 
Pravin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7f6rX-P2STNFU%2BW0iZRbSq9uN8veyWzk4%3D9v4ghgTSTCg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1724425195.3164246.1662365871731%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7e32ccR2tYx%2B4LuiBQuV0m_ocL%3DZwHSuocqAu%2B7N9K6yA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...