Thursday, September 8, 2022

Re: [MW:33451] Tube to tube sheet WPS qualification

 Hello Sujit,

You shall refer ASME section IX Article-1 (QW-193) for tube to Tubesheet tests.

Thanks & Regards
Shahil Saini 

On Thu, Sep 8, 2022, 08:29 sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,

Greeting for the day.

Please guide me regarding tube to tube sheet WPS Qualification.

We are having 8'' and 20'' flange and
 tube size 12mm Od 
thickness of the tube is 0.9 mm


Best regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMNorSJkBUKcBAS3_iwzbejVXnY0sSFL33yk4yxD7k46w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8TFOFdwzb0VNs5v7HUkP7rGEAxgdG%2B8ktVovAgLxZKxA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...