Re: [MW:33162] PQR test required

RT is not mandatory according to ASME sec IX. 

1. It is to help you for destructive testing sampling you can discard the defective location.
2. Most of the customer expects RT examination
3. Additionally you have an provision to prefer UT in lieu of RT

On Mon, 20 Jun 2022 at 12:11, Manoj Singh <manoj.singh1178@gmail.com> wrote:
Hi Teams,

want to know while qualifying PQR is RT is mandatory if use pls. give reference.



Regards 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPkJdRLq5NgcUuh8B6c-s7C7iJCs36LvizYGMY%3Dmx_u%2BiAF8jA%40mail.gmail.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK'S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let's come together as a nation so that they don't have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2k%2BVGDHrJwvCMQ8mNt%3DFAik6Ksa3XkJ%2BvxMZmy%3Drf4DMg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...