QW 409.4 for supplementary essentials on change in Current/Polarity, when referring code call impact testing. This is exempted for ASS, Al, Ni base alloys for change in Current/Polarity.
This essential variable are applicable other than exempted material. This Exemption is not for other base materials due to metallurgical changes taking place while welding.
So not necessary to do toughness if referring code does not calls, and, temp also
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Mon, Jun 13, 2022 at 8:53 AM Mohd Siraj <mohd52100@gmail.com> wrote:
dear,P8 material can be used up to -195C without any impact testing...lests know why you conduct impact testing?--On Wednesday, June 8, 2022 at 8:22:15 AM UTC+3 Yael Nieto wrote:I have a misgiving wiht QW-409.4ASME Section IX Ed 2021 describes:QW-409.4 A change from AC to DC, or vice versa; and in DC welding, a change from electrode negative (straight polarity) to electrode positive (reverse polarity), or vice versa. This variable does not apply to a WPS qualified for welding base metals that are assigned to P-No. 8, P-Nos. 21 through 26, and P-Nos. 41 through 49.I have a base metal P8-P8 WPS, so I know if the construction code requires impact testing for base metal(s) or weld metal, then the for the WPS the variable is supplementary essential but my base metal is P8, also aply ?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aecd6c4d-06a1-4742-ad3b-c1e3c2c51a92n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM8jQzR1%3DUzOiFwPoM%2B0MCacjf%3DsX0Ro4QGn2uqnay1NA%40mail.gmail.com.
Comments