Friday, June 24, 2022

[MW:33175] Consumable insert (QW 404.22) vs preplaced fillermetal (QW 404.58)

What is difference between Consumable insert (QW 404.22) and preplaced fillermetal (QW 404.58) in ASME BPVC Sec IX?
Consumable inserts that conform to SFA-5.30 (ASME BPVC IIC), where as no such refrence or difinition for preplaced fillermetal.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/aa6754a6-c2c8-4aa7-ab0d-cfa77efa4905n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.