Hardness test requirements, is it required as per code or Project specification requirements
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE, CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer.
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Fri, Jun 17, 2022 at 7:53 PM Rameshbabu B <rameshbabu.b@zetwerk.com> wrote:
Hi Sujit,Referring to QW-451.1 the following tests shall be conducted.2 Transverse tensile2 Root Bend2 Face bendAdditionally, you can advise the laboratory to perform a hardness test for Base, Weld, and HAZ which is common when qualifying a PQROn Fri, Jun 17, 2022 at 6:03 PM sujit kumar <sujitkumar19942@gmail.com> wrote:Hii Experts,hope all is well.I want to know which test is required for WPS and how many tests are required as per ASME section IX.?PLATE SPECIFICATION-SA516 GR70PLATE THICKNESS-10MMFILLER USED-ER-70S2ELECTRODE USED-E-7018TOUGHNESS TEST NOT REQUIREDBest regardsSujit Kumar--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0d00b35e-1d18-400f-9bf6-a9a55001f9a0n%40googlegroups.com.
--Ramesh Babu Balaram
Corporate Head, Quality
The Oriental Towers, No. 461, 1st Floor, 17th Cross Road, 4th Sector,
Sector 4, HSR Layout, Bengaluru, Karnataka 560102.
M 9840531355 E rameshbabu.b@zetwerk.com W zetwerk.com
Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hard copy.
This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message --
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2mOnqEbUYXM%2Bt4jZ9hgrOGD-nObkLesQ1%2BGgmyTDZWgAA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOE2QFhk%2BtDZn-BWDerVf86PbJsXZmAp3sBgESBWyB-3Q%40mail.gmail.com.
Comments