Referring to QW-451.1 the following tests shall be conducted.

2 Transverse tensile
2 Root Bend
2 Face bend

Additionally, you can advise the laboratory to perform a hardness test for Base, Weld, and HAZ which is common when qualifying a PQR


On Fri, Jun 17, 2022 at 6:03 PM sujit kumar <sujitkumar19942@gmail.com> wrote:
Hii Experts,

hope all is well.

I want to know which test is required for WPS and how many tests are required as per ASME section IX.?

PLATE SPECIFICATION-SA516  GR70
PLATE THICKNESS-10MM
FILLER USED-ER-70S2
ELECTRODE USED-E-7018
 TOUGHNESS TEST NOT REQUIRED



Best regards
Sujit Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0d00b35e-1d18-400f-9bf6-a9a55001f9a0n%40googlegroups.com.


--

Ramesh Babu Balaram

Corporate Head, Quality

The Oriental Towers, No. 461, 1st Floor, 17th Cross Road, 4th Sector,

Sector 4, HSR Layout, Bengaluru, Karnataka 560102.

M 9840531355  E rameshbabu.b@zetwerk.com  W zetwerk.com

App Green Footer Image Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hard copy.



This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2mOnqEbUYXM%2Bt4jZ9hgrOGD-nObkLesQ1%2BGgmyTDZWgAA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...