[MW:33130] WPS and PQR

Dear all


I have PQR Cs to inconel with impact. 
Thinkness 11.07mm
Deposit weld metal thickness: gtaw-6mm smaw -5.07

I need prepare wps for gtaw only
What thickness range will mention for base metal in wps

Regards 
Saleem 
--
Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omus16kTLJtHK5K7_SZLgZWZTOTV2MdscgWvTiL9Kh%2BW9g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...