Wednesday, December 29, 2021

Re: [MW:32718] Re: requalification of PQR

No issue.
Ensure that Mn content is less than 1.6 % before purchasing.

On Wed, 29 Dec 2021, 09:05 mahesh chilukamari, <chilukamarimahesh@gmail.com> wrote:
Hi,
its a change of classification which is a supplementary essential variables , you can use the filler as proposed and it doesn't require to requalify the PQR if there is no impact test requirements.

On Saturday, 25 December 2021 at 14:44:42 UTC+8 Inspection engineer wrote:
Greetings

Please kindly advise me whether a requalification of PQR is required when changing from ER-70S2 TO ER-70S6.

Since I have a WPS qualified with ER-70S2+E7018. However, due to the non-availability of ER-70S2 can I use ER-70S6 without qualifying for new PQR.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4de450b4-dab0-46b6-bb58-2d0aad16243fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3NipKsWqVUCCNaU9VGSE5Xp_6jAywKg0SG6ORUzBvY9ZQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...