Re: [MW:32717] QW 200.4: Combination of Welding Procedures

Check the GTAW process thickness ranges qualified in PQR and if the combination WPS is within this qualification range then you can use it.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 29 December, 2021, 07:41:40 am GMT+4, Sudhakar Kuppuswamy <sudhakarceng@gmail.com> wrote:


Hi,


Currently one of my clients is having an ambiguity in applying the requirements of ASME Section 09 Clause QW 200.4: Combination of Welding Procedures, Subclause:  a & b requirements. Hence, support is required in finding an interpretation from ASME Section 09. (Interpretation in CS connect is not apparent for this clause)

Background: Two PQRs were qualified separately, PQR A is qualified with SAW process using 8 mm thickness plate and PQR B is qualified with SMAW process using 8 mm thickness plate.

Question: While combining the two PQRs to weld a plate with thickness(es) ranging from 1.5 mm to 16 mm.

Do as per QW 200.4, it is necessary to have the root pass process PQR need to be qualified on a minimum 13 mm thickness plate?

I'm pretty sure it is not required to have a root pass process PQR with minimum 13 mm thickness in the above case. However, it would be helpful if you found any interpretation on this.


Regards,

Sudhakar K CEng MWeldI,IWE.

Welding & Metallurgical Engineer,

Email: sudhakarceng@gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABF8NYVXu5Nu5k5yKnxevQH8xhLhEqjw0Fw7z0ogm--MNr-F-A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...