Thursday, December 9, 2021

Re: [MW:32658] Acceptance criteria for PMI of dissimilar metal weld

Dear Mr. Govindan, 

Do you mean in this case, acceptance criteria shall be in red color as below ? 

6Mo weld to 6Mo
Cr Ni Mo
A312 S31254 (6Mo) 19.5-20.5 17.5-18.5 6-6.5
A312 S31254 (6Mo) 19.5-20.5 17.5-18.5 6-6.5
ERNiCrMo-3 20-23 58 min 8-10
Weld metal required 19.5 17.5 6



Vào Th 5, 9 thg 12, 2021 vào lúc 13:25 Perumal Govindan <perumalgovindan@gmail.com> đã viết:
While welding dissimilar materials, usually lower grade properties shall be acceptable and its a normal industrial practice.

For more information, pease refer your welding specifications of.your project.

Regards 
P Govindan 

On Thu, Dec 9, 2021, 11:39 AM anhtrangnghieng <anhtrangnghieng@gmail.com> wrote:
Dear Experts, 

We have a welded joint: stainless steel type 6Mo UNS S31254 using filler metal ERNiCrMo-3. What would be the chemical requirements criteria ( Cr, Ni, Mo)  be for PMI on this joint? Any standard/ code for reference? 

--




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADOyxJi%2BOSmeuJhmc8e-hvB8c8hMHnzXBMAkX8WuJ9tzJhdrnw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9d6KtR%3Dy-%2BggtZoFBRrAHxA%2BvmuOz4x5pnsHn%2BMDAQhKQ%40mail.gmail.com.


--




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADOyxJhrsUFqzK48SoWsjLmhvxt3ytGgE8m9JxNks%2BeFhC6nug%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...