Worst area where IQI placed and Sensitivity achieved in that particular area
to 
Best area where IQI placed density check. 
where us densitiy range -15% to 30%
Thank you, 
Regards, 
S.SENTHILKUMAR
                      On Friday, 3 December, 2021, 08:44:07 am IST, SEN SEN <senins054@gmail.com> wrote:                  
                  Dear experts
    while doing film interpretation, which all area need to be checked for density with densitometer? spec says 1.8 to 3.5, is it only for weld area or also for entire area of film? please clarify with  which code,
thanks with regards,
senthil P