Re: [MW:32630] HDPE pipe joint (welding), procedure and acceptance

Hi Zakaria.

Based on the Section IX HDPE welding procedure mentioned below/For sample only.




On Thu, Dec 2, 2021 at 7:16 AM TQM <zakaria.ghrab@gmail.com> wrote:
Dears,

  Could you please inform for HDPE pipes joining, if any Welding procedure is required (Is it mandatory as the steel welding case ?) 
the inspection method ?

and the related code/ standard please.

Thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0655b142-a5e8-49de-858d-978316cbe548n%40googlegroups.com.


--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     WELDING ENGINEER,
     BLACKCAT ENGINEERING  WLL,
     DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALhxBzichuf51g8yeA0QvDeBzk8%2BLVHuLznLNdQ-AKKDqHcN3w%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...