Hi Zakaria,

You need to look under this chapter, chapter Off-white is all about Fusion of Plastics. Fusion not Welding is not the term used for joining of  plastics.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Consulting Welding & Metallurgical Engineering Specialist

Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

From: TQM <zakaria.ghrab@gmail.com>
Sent: December 1, 2021 7:19 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: HDPE pipe joint (welding), procedure and acceptance

 

Dears,

 

  Could you please inform for HDPE pipes joining, if any Welding procedure is required (Is it mandatory as the steel welding case ?) 

the inspection method ?

 

and the related code/ standard please.

 

Thank you.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...