Re: [MW:32614] Which Filler wire to be used in between P43 (Inconel 625) to P8 (A240 310S) by GTAW)

inconel 625

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Nov 23, 2021 at 2:14 PM rahmat khan <mkrahmat11730@gmail.com> wrote:
Dear All,

Please help me with this:

1) which filler wire is to be used for GTAW welding of two dissimilar materials P number that is P43 (Inconel 625) to P8 (A240 310S).

2) For SA 516 Gr 70 22mm thick. Ellipsoidal 2:1 dish end, which heat treatment to be used as per ASME Sec VIII Div I UCS 56 After cold forming of dish end.

Please help me I this?

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/441df1fa-c04c-4f4a-a027-af6c169e7cc3n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePjWq7th-zPk1n18Xxj01O2xNouUCJFQpHmWAT4ePm%2BNw%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...