How much flared dia from to which dia
What is % ?
On Thu, 11 Nov 2021, 08:41 Raja Pandiyan, <krajapandiyan@gmail.com> wrote:
Dear experts,--Pl clarify the heat treatment requirements for SA106 Gr.B pipe I.D to be flared and done by hot formed operation like red hot heating with hammering of die in the pipe id to get the required dimensions.Does it require heat treatment?Also the above said process is good engineering practice for flaring operation of pipe?
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADuMvPb%3DddCgS030uK6pZaqS5KnVyeHMG41Vp-rZo29%3DzRAT4w%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3POvW2Jf2Dwbdq5aM3Wp8s3djopP0X_YP1PyL-TTzvMYw%40mail.gmail.com.
Comments