Re: [MW:32593] Alternative MOC - SA387 + SS.304 cladding to complete SS.304

NO.S.S.304 WILL NOT STAND WITH HEIGHT TEMPERATURE SERVICE 

THANKS AND REGARDS 
SUSHIL GAUR 
M.NO.9530278378 

On Sat, Nov 6, 2021 at 7:19 PM uday prabhu <uday31@gmail.com> wrote:
Dear Experts,

Vessel MOC = SA387 GR F11 CL2 + 3mm SS.304 clading
Max operating Temp = 425 C
Max Pr = 20 bar (g)

Can we replace above moc with SS.304.
Will there be Sensitization issues a this temp ??

Regards,

Uday Prabhu

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb883ea1-ba79-407e-a7bc-5197397e0496n%40googlegroups.com.


--

sushil gaur

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAKVvO_U6ex-Pwdyu3T80HfJVfX29mcZvwrXiL7jOUuo-s7DeQ%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...