Dear Experts,                  

During  cladding using  Hasteloy C22 consumable  on reaction chamber roll with base material 1.4776/ 30%CrMo steel 

we immediately noticed during a small test clad, cracks (a lot). as per picture 

Pls advise me what we could do to avoid cracks?


Best Regards 

Neilashkumar P 

--