Mill tolerance for the seamless pipe is 12.50% and 0.3mm for the welded pipe.
-- Whereas Mill tolerance for the seamless/welded fitting & flange is 12.50%
Is standard more stringent in case of welded pipes ?
Please justify.
Regards
Rishabh
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFH_NRKqdyNRYK3bwDnKgd%2BUBHaXDQF6o1WMVfkhTNxNJrNEpw%40mail.gmail.com.