[MW:32594] RE: Alternative MOC - SA387 + SS.304 cladding to complete SS.304

Hi Uday,

 

Choice of S.S 304 may be correct for the said design temperature(425 Deg C). In order to keep the IGC/ sensitization factor under control use 308L welding consumables/fillers would be advisable.

 

It would be good to know what's the process fluid involved? If the process fluid is aggressive, then a switch to SS 316/316L would be a better choice. This would be a process engineer/metallurgical engineers' call to select 304 or other alternatives (316/316L) as needed.

 

Thanks

 

Pradip Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Engineering Specialist

Saudi Aramco Approved Designated Project Welding Engineer (DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

Austenitic Stainless Steel Sensitization | Austral Wright Metals

From: uday prabhu <uday31@gmail.com>
Sent: November 6, 2021 8:46 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: Alternative MOC - SA387 + SS.304 cladding to complete SS.304

 

Dear Experts,

 

Vessel MOC = SA387 GR F11 CL2 + 3mm SS.304 cladding

Max operating Temp = 425 C

Max Pr = 20 bar (g)

 

Can we replace above moc with SS.304.

Will there be Sensitization issues a this temp ??

 

Regards,

 

Uday Prabhu