Skip to main content

[MW:32442] RE: 32439] Re: 32434] Welder Engagement in WQT

Hello Asif,

 

Sorry I got mixed up with the year of publication . This provision was incorporated in API 1104-2020 version. API terms this option as Brother-in-Law welding. See the extracts of the relevant pages. More can't be shared in a public forum. If your contract specifies API -2018 to be followed, legally you can't choose this option, as API 2018 does not address that. However, if allowed by the Authorized Inspector& and the client it's possible. Get the full version of API 1104, 2020 and get your issue straightened.

 

Hope this would help.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Consulting Welding & Metallurgical Engineering  Specialist

Saudi Aramco Approved Designated Project  Welding Engineer(DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@rogers.com,pradip.goswami@gmail.com

Cell/Whasapp:1-905-9793232

 

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Engr. Asif Chowdhury
Sent: July 5, 2021 6:42 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:32439] Re: 32434] Welder Engagement in WQT

 

Dear Mr. Pradip Sir,

 

With all due respect, I didn't find any clause as mentioned in  6. Qualification of Welders as described by you.

 

Could you please tell me in which edition I should look into? As i have gone through API-1104 21st Edition/2018.

 

As I have to reply to my consultant with strong reference about this It would do great for me If you please help me in this case.

 

.Looking forward for your kind reply.

 

Thanks in Advance,

Md. Asif Al-Istiaque Chowdhury

Construction Manager

BRS Gas Transmission Pipeline Project, Bangladesh.

 

On Monday, July 5, 2021 at 10:37:54 AM UTC+7 pgos...@rogers.com wrote:

Hi Asif,

 

API 1104 allows this option. You should engage 2 welders max at a time.

In option 1- One welder welds the GTAW, full pass or more up to the required despot thickness , rest of the passes done by another welder by SMAW process

Option-2 Put 2 welders back-to-back, each weld half of the circumference as explained below, Both uses GTAW(root) + SMAW fill passes.

Refer Clause 6.1 of API 1104-2018, as below. However, these're the pros and cons as explained for both the welding techniques involved..

 

 

The problem one may face:-

 

Hope his would help you to move forward.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Consulting Welding & Metallurgical Engineering  Specialist

Saudi Aramco Approved Designated Project  Welding Engineer(DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of Engr. Asif Chowdhury
Sent: July 4, 2021 6:09 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:32434] Welder Engagement in WQT

 

Dear Experts,

 

With due respect, please read following as I am in deeply need of expert's advice:

 

we have established a WPS with NDT and Destructive test requirements as per API 1104 which is approved by each concerned authority of my project.

 

Our test coupon Dia: 30 inch and Thickness: 25.4 mm

Welding Process: GTAW+SMAW

 

Our client consultant wants us to do WQT as One welder will do One Joint. But We have done several projects in Gas Transmission Pipeline where we have used 02 Welders for Test pieces like this during Welder Qualification Test. It seems really difficult to engage 01 welder for 01 Joint/test piece to Qualify. 

 

Now, our Client Consultant wants reference code or standards in writing which can establish my proposal to use 02 Multi Welders for 01 Joint/test piece during Welder Qualification Test.

 

Also, I want to include several SMAW welders and for that I require to engage 04 welders (02 GTAW Welders+02 SMAW welders) during WQT for 01 joint/test piece.

 

If possible, please help me in this issue as I don't have very much knowledge about ASME 31.8, Sec IX and API 1104. I really have to establish valid point with reference code and standards in order to do the WQT by 02 welders (GTAW+SMAW) and some joints by 04 Welders (02 GTAW+02 SMAW). I request urgent help and kind cooperation with clarification for this issue from the experts in this group.

 

Hoping to have all of yours kind notice and help.

 

Thanks in Advance,

Md. Asif Al-Istiaque Chowdhury

Construction Manager

BRS Gas Transmission Pipeline Project, Bangladesh.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/219b4deb-abdf-4218-b157-81dee64726bbn%40googlegroups.com.

 

Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/10f238d4-3aa1-4d3c-b3c7-785f1cbcfb66n%40googlegroups.com.


Virus-free. www.avg.com

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...