Thursday, September 10, 2020

Re: [MW:31420] SS446 to SS446 (GTAW)

You should go to a super austenitic filler metal which is going to provide higher ductility. What is the working environment of the weld?

Στις Τρί, 4 Αυγ 2020 στις 8:10 μ.μ., ο/η Prasad <prasadloke27@gmail.com> έγραψε:
Dear Sirs,

Greetings !

We are in process to perform WPS/PQR for SS446 to SS446 combination.
Welding done on 20 mm thick plates using ER430 filler.

Test coupon passed for Tensile test but it is getting failed in Bend test .
Need your expertise opinions /suggestions  to complete this WPS/PQR with satisfactory results as per requirements of ASME Section IX .
Especially guidance  to pass Bend test .

Thanks in Advance

Regards
Prasad Loke

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3c8b9b28-f799-4ad7-a21e-d4a5d7e9c4b7o%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BAVw4CcSCqv-spvTBdm3dzR%2Bm7zzYLs%2BeyfPBQAi%2BsgQ%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...