Dear Sir ,
Construction Code Is ASME SEC. VIII Div I.

On Mon 14 Sep, 2020, 8:05 AM 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Design Construction code?

Regards, S.SENTHILKUMAR


On Sunday, 13 September, 2020, 10:49:50 am IST, Patel Ankit <aapatel271@gmail.com> wrote:


Hello Team,

I hope all member will be fine & Healthy.

My question is How can define take radiography full or spot.

In my drawing no any data mention about radiography like (Full, Spot , No joint efficiency ).

Sir pl. Tell me if you have any reference.

Thanks,
Ankit Patel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuzvCnHn-T5C2T%2BxVHLv7NwMSj3eJoSz6o3rfZY-%2BTsdMg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1200134180.1249169.1600010539405%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-Puy9OrWvP%2By1KV%2BUYuiLnUoBpVmTAD-duJMGE_UPFUMT%2Bg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...