If the Code is ASME VIII-1 the spot radiography is defined in UW-11(b) and in UW-52.
However, you have to consider the UW-12 and take into account the joint efficiencies of the butt welds and the joint efficiency of seamless vessel sections like heads.
Depending on the extend of the RT you stamp either RT 2 or RT 3 on the name plate


Στις Κυρ, 13 Σεπ 2020 στις 8:19 π.μ., ο/η Patel Ankit <aapatel271@gmail.com> έγραψε:
Hello Team,

I hope all member will be fine & Healthy.

My question is How can define take radiography full or spot.

In my drawing no any data mention about radiography like (Full, Spot , No joint efficiency ).

Sir pl. Tell me if you have any reference.

Thanks,
Ankit Patel

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALR-PuzvCnHn-T5C2T%2BxVHLv7NwMSj3eJoSz6o3rfZY-%2BTsdMg%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Dck5jd9LUi_K3gqz8c-bY8qX7oWpn%3DOY512W%2BkihVzvQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...