Re: [MW:31457] Welder qualified 2 7/8 OD, whether he can weld 2” NPS

Dear Murali,
Welder is not eligible for 2".
Should be done separately.

On Wed, 9 Sep 2020, 06:57 Murali Krishnan, <muraligkrishnan@gmail.com> wrote:
Greetings,

I have a weldolet 2" NPS X OD 82 mm, I want to use the welder qualified for 2 7/8 (73 mm) & over.

Query initiated by client that as per ASME SEC IX Table QW 452.3 foot note (b) states that 2 7/8 in. (72mm) O.D. is the equivalent of NPS 2 1/2 (DN 65). In this case the welder client says welder is not qualified for 2 inch NPS.


since the welder qualification essential variable is OD inline with ASME SEC IX, kindly advice.

If any reference kindly share the same.

Thanks 
Murali


--
 
 
Thanks and Best Regards,
 
G.Murali krishnan
Mob : +966-501487307
Saudi Arabia

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANtiPKs%3D8_skdC4DU-H0__v9sE3CT7tq9RP0D-_RV%2B7OOuybNQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANii3RNa0JO3mEj3jSdeCjwb5wBVNbVB-uzSx1Z-EN%3DFNboYDw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...