Re: [MW:31502] Welding Metallurgy-Weldability of High Carbon Steels

You  could weld them using the same method for welding cast iron.
I have done it and it works

Στις Τρί, 22 Σεπ 2020 στις 10:58 π.μ., ο/η Zacharias Rohith Joseph <rohithjoseph18@gmail.com> έγραψε:

High Carbon Steel is characterized by as having what type of weldability?

1.Very Good Weldability

2.Not Weldable

3.Good weldability with SMAW process

4.Good Weldablity

5.Poor


Can the IWE's in the group pls explain why the answer to this question is option 3? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c75217b8-a8e8-4ddc-93f6-aafbdb137defn%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40AnRUJFqNCT3rZ-wnj80Xu2F%2BugYkMhfB_w_OQDX2s1Fw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...