[MW:31481] ASME BPV Sec VIII div1 , UCS-68(b) - PWHT requirements

Can you please provide your interpretation for the following requirements of UCS-68(b)
Vessel MDMT - 48 °C , PWHT - not required

In accordance with para UCS-68(b) PWHT is required except for Category A and B joints with 100% RT, lightly loaded attachments and seal welds only.
and it is silent on category C , D welds and other attachments.

Question: does this mean PWHT is required for Category C and D, even though it is exempted for Category A and B welds? then vessel will undergo local PWHT
In my opinion we should not interpret this way and look for only what is code specifies (i.e. if Category A and B or other welds as specified is exempted entire vessel is exempted)  

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVub%3DX04JD0J0AhOJ9qN7%2BRpXo1ybR0CJPxEM8Qv%3D1OvwUdA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...