Re: [MW:31515] ASME Material Re-certification

if marking is available than very good.simply go for mechanical and chemical test.you should ensure all chemical element should be reported in report given in spec chemical table. 
if in qcp final document is MTC may be NCR raise for this.

On Tue, 22 Sep 2020, 11:17 am Rejoy Thomas, <rejoythomas90@gmail.com> wrote:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k-Or55X3fF5Yzg5YZ11BdcaPsVCV7ZHsO-u4gWGy7-%2BBw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...