Re: [MW:31377] Unlisted Material AWS D1.1

U can contact material for welding procedure. They give some inputs which will be useful. Generally root Welding is done under match filler metal and other layer matched filler material. Preheat is based on thickness and CE. Over preheat will reduce the Hardness. This is not coming under preview of D1.1, u can follow it's procedure. 

On Tue, 1 Sep 2020 1:45 am , <pgoswami@rogers.com> wrote:

Hardox, is an abrasion resistant steel, not very commonly used for structural fabrication. Here're two data sheets which tells almost the same story .

 

Welding   considerations for this steels are quite tricky and requires very high level of preheat .  To the best of my knowledge structural codes does not incorporate use of such abrasion resistant  steel. If this material is acceptable for construction you should ask the WPS to supported by a qualified PQR form welding approval  prior to production.

 

Thanks.

 

 

Pradip Goswami, P.Eng, IWE

Consultant-Welding-Metallurgical Engineering

 

Cell & Whatsapp-905-9793232.

Personal:pgoswami@rogers.com

 

 

 

 

 

From: Kannayeram Gnanapandithan <kgpandithan@gmail.com>
Sent: August 31, 2020 11:53 AM
To: materials-welding <materials-welding@googlegroups.com>
Subject: Re: [MW:31373] Unlisted Material AWS D1.1

 

Only hardness other strength not guaranteed

 

On Mon, 31 Aug 2020 8:14 pm Vishwas Keskar, <vvkeskar123@gmail.com> wrote:

Request them to furnish Mechanical properties

They will furnish 

No issue at all 

 

On Mon, 31 Aug 2020, 18:27 jaimin...@gmail.com, <jaiminthejack@gmail.com> wrote:

Dear Gents,

 

I got one WPS for  hardox 450 

 

Required Code: AWS D1.1

Plate Thk: 25mm

 

My concern is that as per given Data sheet there is not specified Tensile Strength ,on what basis we can accept Report of Tensile Test?

 

This is my first experience with unlisted material.

 

Thanks & Regards

Jaimin Patel
B.E Mechanical

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/46b74d37-8ccf-40dd-ab4e-dda0b27073e7n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3OM-KTP9YMPK2gWcMKsEBAj8uOwvhjw4HuHRpowW4Jn%3Dg%40mail.gmail.com.


Virus-free. www.avg.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAAhissbuC7PQrXdaBlEBjUVAQAAAAA%3D%40rogers.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNVWE6_2mXd9bR8EfJGcAPbjztaV-2Re6yTSrk-6fQp1Q%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...