It is important that you describe what code you are using, each standard has its advantages and limitations.
El dom., 26 jul. 2020 a las 9:19, Venkat Ramana (<venkatgps.ramana@gmail.com>) escribió:
Hi Experts,--My query is once welder was qualified for CS material, can he weld for SS also....Please advise
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsN5Yzfq036c3S4fumVeSKUo8HgZxbpkSu-daMchAShF5w%40mail.gmail.com.
Ing. José Juan Jiménez Alejandro
Independent Consultant in Parts
and Pressure Equipment
SSI-TPI
Móvil +52 1 812 352 4606
Skype: jjjimeneza
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurJ0PzACcC%2BVD%3DJnqHFkzO7s6ykJ0N%3DD8SABNia2xL40Wg%40mail.gmail.com.