[MW:31157] Re: WPS qualified in 5G and Welder qualification required in 6G

As API 1104 specifications

From
Herish varude
Mob.No.:-7990746918

On Mon, Jul 20, 2020, 10:17 AM HARISH VARUDE <harish.varude02@gmail.com> wrote:
Dear all,

Contractor have a Approved WPS in 5G position and now he want to do weld joints in 2G position and also want to welder qualification in 6G position.
Can it possible???

From
Herish varude
Mob.No.:-7990746918

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGP-YK%2B69MY7CMiRy1yKR2gKcD%2B-W4r%2B1RCNBU%3DNvZ%3D6simwHw%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...